Chromium-Aluminide Coatings on Inconel 718 Alloy and Fe-Cr-Ni SuperAlloy
Yıl: 2019 Cilt: 23 Sayı: 5 Sayfa Aralığı: 817 - 823 Metin Dili: İngilizce DOI: 10.16984/saufenbilder.495407 İndeks Tarihi: 26-11-2019
Chromium-Aluminide Coatings on Inconel 718 Alloy and Fe-Cr-Ni SuperAlloy
Öz: In this study, it is invastigated the low-temperature chromium aluminide coatings on a FeCrNi-basesuperalloy and Inconel 718 by pack cementation method. Pack-aluminizing diffusion coating was appliedat 800°C during 4 and 6 hours. The chromium-aluminising powder packs were prepared using aluminiumand chromium powders as a source for depositing aluminium and chrominium, Al2O3 powder as an inertfiller and ammonium chloride NH4Cl as an activator. SEM (scanning electron microscope) EDS withenergy dispersive X-ray spectrometer and XRD were used to characterize the coating layers. SEM analysisrevealed that coating layers were homogenous, compact and nonporous and there was a good bonding atthe interface of the coating and matrix. Layer thickness variation was changed from 11 to 18 μm measuredfrom the surface to the matrix. The hardness of the coating layer increased to 1000 HVN while the hardnessof the matrix was 340 HVN with the increasing process time.
Anahtar Kelime: Belge Türü: Makale Makale Türü: Araştırma Makalesi Erişim Türü: Erişime Açık
- I. Schoukens, I. Vandendael, J. De Strycker, A. A. Saleh, H. Terryn, and I. De Graeve, “Effect of surface composition and microstructure of aluminised steel on the formation of a titanium-based conversion layer,” Surface and Coatings Technology, vol. 235, pp. 628–636, Nov. 2013.
- Z. D. Xiang and P. K. Datta, “Relationship between pack chemistry and aluminide coating formation for low-temperature aluminisation of alloy steels,” Acta Materialia, vol. 54, pp. 4453–4463, 2006.
- R. Pillai et al., “Carbides in an aluminised single crystal superalloy: Tracing the source of carbon,” Surface and Coatings Technology, vol. 288, pp. 15–24, 2016.
- A. Erdogan, “Investigation of high temperature dry sliding behavior of borided H13 hot work tool steel with nanoboron powder,” Surface & Coatings Technology, 2018.
- M. Sabri, A. Erdogan, M. Öge, and A. Günen, “Dry sliding wear behavior of borided hot-work tool steel at elevated temperatures,” Surface & Coatings Technology, vol. 328, pp. 54–62, 2017.
- D. Chaliampalias et al., “The effect of Al and Cr additions on pack cementation zinc coatings,” Applied Surface Science, vol. 256, no. 11, pp. 3618–3623, Mar. 2010.
- Y. F. Yang, C. Y. Jiang, Z. B. Bao, S. L. Zhu, and F. H. Wang, “Effect of aluminisation characteristics on the microstructure of single phase β-(Ni,Pt)Al coating and the isothermal oxidation behaviour,” Corrosion Science, vol. 106, pp. 43–54, 2016.
- K. Nikolov, P. Kaestner, C. P. Klages, S. Puls, and B. Schuhmacher, “Low-pressure diffusion chromising of thin low-carbon steel sheet for improved surface and bulk properties,” Journal of Alloys and Compounds, vol. 692, pp. 101–107, 2017.
- F. J. Pérez, F. Pedraza, M. P. Hierro, M. C. Carpintero, and C. Gómez, “Chromising of stainless steels by the use of the CVD-FBR technology,” Surface and Coatings Technology, vol. 184, no. 1, pp. 47–54, 2004.
- X. J. Lu and Z. D. Xiang, “Formation of chromium nitride coatings on carbon steels by pack cementation process,” Surface and Coatings Technology, vol. 309, pp. 994– 1000, Jan. 2017.
- Z. D. Xiang and P. K. Datta, “Pack aluminisation of low alloy steels at temperatures below 700 °C,” Surface and Coatings Technology, vol. 184, no. 1, pp. 108–115, Jun. 2004.
- Yener, Tuba. 2019. “Low Temperature Aluminising of Fe-Cr-Ni Super Alloy by Pack Cementation.” Vacuum 162 (September 2018). Elsevier: 114–20. doi:10.1016/j.vacuum.2019.01.040.
APA | YENER T (2019). Chromium-Aluminide Coatings on Inconel 718 Alloy and Fe-Cr-Ni SuperAlloy. , 817 - 823. 10.16984/saufenbilder.495407 |
Chicago | YENER Tuba Chromium-Aluminide Coatings on Inconel 718 Alloy and Fe-Cr-Ni SuperAlloy. (2019): 817 - 823. 10.16984/saufenbilder.495407 |
MLA | YENER Tuba Chromium-Aluminide Coatings on Inconel 718 Alloy and Fe-Cr-Ni SuperAlloy. , 2019, ss.817 - 823. 10.16984/saufenbilder.495407 |
AMA | YENER T Chromium-Aluminide Coatings on Inconel 718 Alloy and Fe-Cr-Ni SuperAlloy. . 2019; 817 - 823. 10.16984/saufenbilder.495407 |
Vancouver | YENER T Chromium-Aluminide Coatings on Inconel 718 Alloy and Fe-Cr-Ni SuperAlloy. . 2019; 817 - 823. 10.16984/saufenbilder.495407 |
IEEE | YENER T "Chromium-Aluminide Coatings on Inconel 718 Alloy and Fe-Cr-Ni SuperAlloy." , ss.817 - 823, 2019. 10.16984/saufenbilder.495407 |
ISNAD | YENER, Tuba. "Chromium-Aluminide Coatings on Inconel 718 Alloy and Fe-Cr-Ni SuperAlloy". (2019), 817-823. https://doi.org/10.16984/saufenbilder.495407 |
APA | YENER T (2019). Chromium-Aluminide Coatings on Inconel 718 Alloy and Fe-Cr-Ni SuperAlloy. Sakarya Üniversitesi Fen Bilimleri Enstitüsü Dergisi, 23(5), 817 - 823. 10.16984/saufenbilder.495407 |
Chicago | YENER Tuba Chromium-Aluminide Coatings on Inconel 718 Alloy and Fe-Cr-Ni SuperAlloy. Sakarya Üniversitesi Fen Bilimleri Enstitüsü Dergisi 23, no.5 (2019): 817 - 823. 10.16984/saufenbilder.495407 |
MLA | YENER Tuba Chromium-Aluminide Coatings on Inconel 718 Alloy and Fe-Cr-Ni SuperAlloy. Sakarya Üniversitesi Fen Bilimleri Enstitüsü Dergisi, vol.23, no.5, 2019, ss.817 - 823. 10.16984/saufenbilder.495407 |
AMA | YENER T Chromium-Aluminide Coatings on Inconel 718 Alloy and Fe-Cr-Ni SuperAlloy. Sakarya Üniversitesi Fen Bilimleri Enstitüsü Dergisi. 2019; 23(5): 817 - 823. 10.16984/saufenbilder.495407 |
Vancouver | YENER T Chromium-Aluminide Coatings on Inconel 718 Alloy and Fe-Cr-Ni SuperAlloy. Sakarya Üniversitesi Fen Bilimleri Enstitüsü Dergisi. 2019; 23(5): 817 - 823. 10.16984/saufenbilder.495407 |
IEEE | YENER T "Chromium-Aluminide Coatings on Inconel 718 Alloy and Fe-Cr-Ni SuperAlloy." Sakarya Üniversitesi Fen Bilimleri Enstitüsü Dergisi, 23, ss.817 - 823, 2019. 10.16984/saufenbilder.495407 |
ISNAD | YENER, Tuba. "Chromium-Aluminide Coatings on Inconel 718 Alloy and Fe-Cr-Ni SuperAlloy". Sakarya Üniversitesi Fen Bilimleri Enstitüsü Dergisi 23/5 (2019), 817-823. https://doi.org/10.16984/saufenbilder.495407 |